Preparation of Ultrafine Oxide Powders by Inductively Coupled Plasma Generated with Modified Conventional Induction Heater
https://doi.org/10.50974/00043319
https://doi.org/10.50974/00043319726fcacb-6e9f-48b8-bbed-4a1888526702
名前 / ファイル | ライセンス | アクション |
---|---|---|
![]() |
|
Item type | 紀要論文 / Departmental Bulletin Paper(1) | |||||||||
---|---|---|---|---|---|---|---|---|---|---|
公開日 | 2008-05-02 | |||||||||
タイトル | ||||||||||
タイトル | Preparation of Ultrafine Oxide Powders by Inductively Coupled Plasma Generated with Modified Conventional Induction Heater | |||||||||
言語 | ||||||||||
言語 | eng | |||||||||
資源タイプ | ||||||||||
資源タイプ識別子 | http://purl.org/coar/resource_type/c_6501 | |||||||||
資源タイプ | departmental bulletin paper | |||||||||
ID登録 | ||||||||||
ID登録 | 10.50974/00043319 | |||||||||
ID登録タイプ | JaLC | |||||||||
著者 |
Kagawa, Masahiro
× Kagawa, Masahiro
× Nagae, Tsuneki
|
|||||||||
抄録 | ||||||||||
内容記述タイプ | Abstract | |||||||||
内容記述 | Ultrafine oxide powders (MgO and ZrO_2, 0.01 μm order of size) were prepared by spraying nitrate solutions into an argon inductively coupled plasma of ultra-high temperature (ICP). A conventional induction heater (5 kw, 400 kHz and thyratron-controlled) was modified for generating the argon ICP flame. The basic modification consisted in increasing its power and frequency (15 kw, 4-16 MHz and thyristor-control led). In order to quench the formed powders rapidly, a water-cooled powder collector was used. The particle shape of the magnesium oxide was not cubic but roundish, and the main phase of the zirconium oxide was metastable tetragonal-ZrO_2. These suggest that the powders formed by ICP should be quenched so rapidly that they could not grow large or could not convert to high temperature phases. The particle size distribution of the magnesium oxide followed the Gaussian type of formula proposed by Aboav (range 0.016-0.044 μm, modal diameter 0.028 μm). | |||||||||
書誌情報 |
Science reports of the Research Institutes, Tohoku University. Ser. A, Physics, chemistry and metallurgy 巻 31, p. 216-224, 発行日 1983 |
|||||||||
ISSN | ||||||||||
収録物識別子タイプ | ISSN | |||||||||
収録物識別子 | 00408808 | |||||||||
書誌レコードID | ||||||||||
収録物識別子タイプ | NCID | |||||||||
収録物識別子 | AA00836167 | |||||||||
フォーマット | ||||||||||
内容記述タイプ | Other | |||||||||
内容記述 | application/pdf | |||||||||
著者版フラグ | ||||||||||
出版タイプ | VoR | |||||||||
出版タイプResource | http://purl.org/coar/version/c_970fb48d4fbd8a85 | |||||||||
出版者 | ||||||||||
出版者 | Tohoku University | |||||||||
資源タイプ | ||||||||||
内容記述タイプ | Other | |||||||||
内容記述 | 紀要類(bulletin) | |||||||||
登録日 | ||||||||||
日付 | 2008-05-02 | |||||||||
日付タイプ | Created | |||||||||
公開日(投稿完了日) | ||||||||||
日付 | 2008-05-02 | |||||||||
日付タイプ | Created | |||||||||
発行日 | ||||||||||
日付 | 1983 | |||||||||
日付タイプ | Created | |||||||||
フォーマット | ||||||||||
内容記述タイプ | Other | |||||||||
内容記述 | 651544 bytes | |||||||||
更新日 | ||||||||||
日付 | 2010-01-27 | |||||||||
日付タイプ | Created |